Solder Bridging: Stencil, Reflow & Wave Root Causes
Diagnose solder bridging across stencil printing, placement, reflow, and wave soldering, then stop shorts with solder mask, thief pads, and pad-safe rework.
Technical dispatches and explainers tagged under #reflow-soldering.
Diagnose solder bridging across stencil printing, placement, reflow, and wave soldering, then stop shorts with solder mask, thief pads, and pad-safe rework.
Through-hole mounting inserts leads through drilled holes; surface-mount parts sit on flat pads and reflow first. Keep plated holes for heavy or mated parts.
Configure Pre-Reflow and Post-Reflow 3D Automated Optical Inspection (AOI) in SMT assembly: Moiré phase-shift optics, IPC-A-610 Section 8 SMD vs SMT thresholds, and 6 OEM platforms.
Reflow soldering stages, the J-STD-020 figures those sheets print, and the peak, ramp, and time-above-liquidus cells left blank.
Wave soldering vs reflow: reflow melts printed paste across the assembly, and a wave wets the underside. Assign each part, then use selective or hand soldering for the rest.