Solder Bridging: Stencil, Reflow & Wave Root Causes
Diagnose solder bridging across stencil printing, placement, reflow, and wave soldering, then stop shorts with solder mask, thief pads, and pad-safe rework.
Technical dispatches and explainers tagged under #wave-soldering.
Diagnose solder bridging across stencil printing, placement, reflow, and wave soldering, then stop shorts with solder mask, thief pads, and pad-safe rework.
Through-hole mounting inserts leads through drilled holes; surface-mount parts sit on flat pads and reflow first. Keep plated holes for heavy or mated parts.
Configure wave soldering equipment across spray fluxing (750–1,500 µg/in²), preheat (95–125 °C topside), and dual-wave SAC305 contact (255–265 °C, 3.0–4.5 s dwell).
Wave soldering vs reflow: reflow melts printed paste across the assembly, and a wave wets the underside. Assign each part, then use selective or hand soldering for the rest.